This study investigates the mechanical properties of geopolymer concrete made with ground granulated blast furnace slag (GGBS) and silica fume (SF) as binders. The influence of varying binder proportions and sodium silicate-to-sodium hydroxide (SS-to-SH) ratios of 1.5 and 2.0 in the alkali-activated solution was examined. Experimental tests evaluated slump, compressive strength, modulus of elasticity, and splitting tensile strength at 1, 7, and 28 days. Increasing SF content up to 50% in the binder with a solution ratio of 1.5 improved the 28-day compressive strength by 50% compared to mixes made solely with slag. However, further increase in SF reduced splitting tensile strength and compressive strength by 79 and 56%, respectively, at 28 days. Increasing the solution ratio from 1.5 to 2.0 enhanced compressive strength for slag-dominant mixes by up to 63% but reduced strength for SF-rich mixes by up to 87%. The highest modulus of elasticity, 18.7 GPa, was achieved with slag-only binders and a solution ratio of 2.0, marking a 240% increase over its counterpart mix with a lower solution ratio. Equal GGBS and SF blends improved splitting tensile strength compared to SF-rich mixes but were surpassed by GGBS-rich mixes in terms of overall structural performance.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC11914085PMC
http://dx.doi.org/10.1038/s41598-025-93637-7DOI Listing

Publication Analysis

Top Keywords

compressive strength
16
solution ratio
16
splitting tensile
12
tensile strength
12
ggbs silica
8
silica fume
8
mechanical properties
8
properties geopolymer
8
geopolymer concrete
8
strength
8

Similar Publications

Bioactive hydroxyapatite-sodium silicate waterglass reinforced with nanocollagen from Chitala ornata fish skin for bone engineering.

Int J Biol Macromol

September 2025

The Materials Engineering Department, Faculty of Engineering, Kasetsart University, Phaholyothin Rd., Bangkok 10900, Thailand. Electronic address:

A prototype bioactive calcium phosphate model-specifically hydroxyapatite (HA) derived from eggshells-was developed using a sodium silicate (NaSiO) solution as an inorganic binder, precursor, and reinforcing agent, in combination with collagen nanofibers for bone engineering applications. The sodium silicate solution, functioning as a waterglass adhesive, introduced cohesive forces within the hydroxyapatite matrix, thereby enhancing its physical, chemical, and mechanical properties. Eggshell-derived bioactive hydroxyapatite offers several advantages, including non-toxicity, biocompatibility, collagen adhesion, and the ability to mimic bone structure, making it suitable for tissue engineering.

View Article and Find Full Text PDF

The use of highly flammable materials such as foams, resins, and plastics has led to an increase in the frequency and severity of urban fires worldwide. To address this issue, this study developed a high-specific-surface-area mesoporous metal-organic framework (Fe-MOFs) with heat trapping and smoke adsorption. The Fe-MOFs, zinc tailings (ZTs), piperazine pyrophosphate (PAPP), and sodium lignosulfonate (LS) were used to modify rigid polyurethane foam (RPUF).

View Article and Find Full Text PDF

The rapid development of flexible electronics has intensified the demand for high-performance energy storage solutions. This research aims to enhance the performance of flexible supercapacitors under extreme temperatures through a lignin cross-linked poly(vinyl alcohol) (PVA) gel electrolyte. By incorporating lignin with PVA and using polyethylene glycol diglycidyl ether as a cross-linker, a hydrogel (PL, represents the mass ratio of lignin to PVA) with an enhanced three-dimensional network structure was constructed.

View Article and Find Full Text PDF

Plastic waste poses environmental and health risks, highlighting the need for sustainable reuse in construction. This study introduces a novel solution to plastic waste utilization by: (1) developing rheological testing equipment from plastic using 3D printing technology, and (2) enhancing the rheological performance of self-compacting mortar (SCM) with 3D-printed plastic fine aggregates (3DPFA). SCM mixtures incorporating 5%, 10%, 15%, and 20% 3DPFA as a replacement for natural sand were prepared and tested to evaluate fresh, mechanical, and thermal properties through mini-slump flow, T20 spread time, J-ring flow, V-funnel, compressive strength, UPV, and thermal conductivity tests.

View Article and Find Full Text PDF

Tumor development is accompanied by strong physico-chemical modifications. Among them, compressive stress can emerge in both the epithelial and stromal compartments. Using a simple two-dimensional compression assay which consisted in placing an agarose weight on top of adherent cells, we studied the impact of compressive stress on cell proliferation and motility in different pancreatic cancer cell lines.

View Article and Find Full Text PDF