The aim of this study was to compare the hardness, chemical composition, and microstructure of various self-ligating ceramic orthodontic brackets and enamel. Sixty ceramic brackets (0.022″ × 0.028″) from six different orthodontic firms (Damon Clear 2, Genius Crystal, Empower 2 Clear, Clarity Ultra, Alpine SL Clear, and Experience Ceramic) were tested using a microhardness tester and a scanning electron microscope (SEM) equipped with energy-dispersive spectroscopy (EDS). The hardness of the ceramic brackets ranged from 1969.8 to 2567.3 VH. The statistical analysis using the Kruskal-Wallis and Mann-Whitney tests revealed significant differences in microhardness between most of the ceramic brackets. Additionally, this study found that passive self-ligating brackets exhibited a significantly higher hardness than that of active self-ligating brackets ( = 0.01). The SEM analysis showed that the variations in the oxygen and alumina composition between the six bracket types were also statistically significant ( = 0.01). Among all of the ceramic brackets tested, Alpine brackets displayed the lowest hardness values, making them a potential choice for minimizing enamel damage. Notably, the hardness of self-ligating ceramic brackets was found to be at least six times greater than that of enamel, raising concerns about their potential to cause trauma to the enamel of antagonistic teeth. Consequently, the researchers recommend avoiding bonding ceramic brackets to the mandibular teeth or elevating occlusion with turbo-bites to prevent traumatic contact during treatment.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC12293928 | PMC |
http://dx.doi.org/10.3390/dj13070285 | DOI Listing |
Materials (Basel)
August 2025
Department of Conservative Dentistry and Periodontology, Jena University Hospital, An der alten Post 4, 07743 Jena, Germany.
In adhesive dentistry, debonding-on-demand is attractive for situations where no permanent attachment is required. Due to its destructive nature, ultraviolet (UV) light may be of interest for attenuating bond forces. The aim of this study was to investigate the impact of UV light on the shear bond strength (SBS) of etch-and-rinse (n = 4) and universal adhesives (n = 3).
View Article and Find Full Text PDFThe aim of this study was to evaluate the shear bond strength and Adhesive Remnant Index (ARI) of ceramic brackets bonded to enamel using a universal adhesive system free of bisphenol A glycidyl methacrylate (Bis-GMA). A total of 100 bovine incisors were divided into 2 groups (n = 50) that received ceramic brackets (Morelli Ceramic or Ice Clear) bonded after acid etching and application of 1 of 5 adhesive systems (n = 10): Adper Single Bond 2, a conventional adhesive system (control group); Scotchbond Universal Plus, a Bis-GMA-free universal adhesive system; and Single Bond Universal, BeautiBond Xtreme, and BeautiOrtho Bond II, all Bis-GMA-containing universal adhesives. Shear bond strength was tested in a universal testing machine (50-kgf load cell; 0.
View Article and Find Full Text PDFBioinformation
May 2025
Department of Biochemistry, Index Medical College Hospital and Research Centre, Indore, Madhya Pradesh, India.
Periodontal and microbiological characteristic among cleft lip and/or palate patients undergoing fixed orthodontic treatment is of interest. Plaque and saliva samples showed high prevalence of (83%), (67%), and (55%). analysis showed significantly greater biofilm formation on stainless steel brackets compared to ceramic brackets (p < 0.
View Article and Find Full Text PDFDent Mater
August 2025
School/Hospital of Stomatology, Zhejiang Chinese Medical University, Hangzhou 310053, China. Electronic address:
Objectives: This study evaluates the feasibility and safety of a laser-induced reversible adhesive (LIRA) by assessing intrapulpal temperature changes (ITC), shear bond strength (SBS) following laser irradiation, and optimal adhesive removal methods.
Methods: Thirty premolars were used to measure ITC under laser powers of 1 W, 2 W, and 3 W until the temperature exceeded the 5.6 ℃ threshold.
Acta Odontol Latinoam
April 2025
Faculdade São Leopoldo Mandic, São Paulo, Brazil.
Aim: During orthodontic treatment, the presence of brackets increases the accumulation of biofilm, which can increase the surface degradation of brackets. Thus, cleaning methods must address removal of both biofilm and stains, specially acquired due to cigarette smoke. Therefore, color change and surface texture of esthetic brackets subjected to cigarette smoke were evaluated before and after use of different cleaning treatments.